A:-Dyeing
B:-Printing
C:-Sizing
D:-Finishing
B:-Printing
C:-Sizing
D:-Finishing
Correct Answer:- Option-D
2:-The main constituent of wool fiber is
2:-The main constituent of wool fiber is
A:-Keratin
B:-Cellulose
C:-Glucose
D:-Lignin
B:-Cellulose
C:-Glucose
D:-Lignin
Correct Answer:- Option-A
3:-_________ is used as a mordant for dyeing cotton with basic dyes.
3:-_________ is used as a mordant for dyeing cotton with basic dyes.
A:-Tanic acid
B:-Acetic acid
C:-Na OH
D:-Sodium carbonate
B:-Acetic acid
C:-Na OH
D:-Sodium carbonate
Correct Answer:- Option-A
4:-The staple length of cotton fiber will be in the range of _______ inches.
4:-The staple length of cotton fiber will be in the range of _______ inches.
A:-15-20
B:-0.4-2.5
C:-7-12
D:-4-6
B:-0.4-2.5
C:-7-12
D:-4-6
Correct Answer:- Option-B
5:-This is a yarn producing machine.
5:-This is a yarn producing machine.
A:-Loom
B:-Ring frame
C:-Jigger
D:-Reel
B:-Ring frame
C:-Jigger
D:-Reel
Correct Answer:- Option-B
6:-An example for a natural protein fiber is
6:-An example for a natural protein fiber is
A:-Cotton
B:-Nylon
C:-Silk
D:-Linen
B:-Nylon
C:-Silk
D:-Linen
Correct Answer:- Option-C
7:-The lea tester is used to determine _______ of yarn.
A:-Evenness
B:-TPI
C:-Strength
D:-Hairiness
7:-The lea tester is used to determine _______ of yarn.
A:-Evenness
B:-TPI
C:-Strength
D:-Hairiness
Correct Answer:- Option-C
8:-The pH of peroxide bleaching is
8:-The pH of peroxide bleaching is
A:-13-15
B:-3-5
C:-6-7
D:-8-10
B:-3-5
C:-6-7
D:-8-10
Correct Answer:- Option-D
9:-Anti-shrink finish is given by
9:-Anti-shrink finish is given by
A:-Embossing
B:-Winch
C:-Sanforizing
B:-Winch
C:-Sanforizing
D:-Drapping
Correct Answer:- Option-C
10:-20 kg of cloth has to be dyed with 2% shade the amount of dye stuff to be taken is
10:-20 kg of cloth has to be dyed with 2% shade the amount of dye stuff to be taken is
A:-400 g
B:-40 g
C:-4 kg
D:-2 kg
B:-40 g
C:-4 kg
D:-2 kg
Correct Answer:- Option-A